Induction Hardness 1.0
EN 10083-2:1998 |
---|
Quenched and tempered steels - Technical delivery conditions for unalloyed quality steels |
Not alloyed quality steel: The content of oxide inclusions is not limited
The maximum content of P and S are higher with respect to the special steels EN 10083-1/3 Poor surface and mechanical fatigue strength of the hardened layer Limited repetitiveness of the heat treatment |
Steel type: |
« back to steel typology selection